Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.73 J/cm | 3.24 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 1.73 J/cm | 3.24 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |