Polymer Property : Izod Impact, Notched = 28.01 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 14.95 J/cm

@Thickness 3.20 mm
28.01 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.
Izod Impact, Notched 14.95 J/cm

@Thickness 3.20 mm
28.01 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 1010R PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 14.95 J/cm

@Thickness 3.20 mm
28.01 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 14.95 J/cm

@Thickness 3.20 mm
28.01 ft-lb/in

@Thickness 0.126 in
reverse notched; ASTM D 256
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..
Izod Impact, Notched 14.95 J/cm

@Thickness 3.20 mm
28.01 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 1010M PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.