Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |