Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel resin. This grade was developed for autom.. |