Izod Impact, Notched 12.5 J/cm
23.4 ft-lb/in
ASTM D256
Spartech Royalite R60M Hi-Impact ABS/PVC Resin
Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are air..