Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 12.5 J/cm | 23.4 ft-lb/in | ASTM D256 |
Spartech Royalite R60M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are air.. |