Mechanical Properties Metric English Comments
Izod Impact, Notched 0.220 - 12.0 J/cm
0.412 - 22.5 ft-lb/in
Average value: 0.998 J/cm Grade Count:29
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..