Mechanical Properties Metric English Comments
Izod Impact, Notched 22.24 J/cm
41.66 ft-lb/in
ASTM D256
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC
QC-8816 is a polyester hybrid engineered structural composite molding compound reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness and fatigue resist..