Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256A
Resinoid 1363 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon
LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant.
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU
LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity.
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus.
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EXT115 PPE+PS (Asia Pacific)
PPE+PS, Auto exterior grade, wax remover resistant
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC
LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.