Polymer Property : Izod Impact, Notched = 2.77 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.77 J/cm

@Temperature -30.0 °C
5.19 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycolac® EXABS01 ABS
Sheet extrusion ABS with medium impact.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC
LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific)
LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RV007ESS PA 66 (Europe-Africa-Middle East)
LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 (Asia Pacific)
LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched 2.77 J/cm

@Temperature 23.0 °C
5.19 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl EN110 PPE+PS (Asia Pacific)
Medium heat, extrusion grade PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX2637 PPE+HIPS (Asia Pacific)
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RV007ES PA 66
LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RX06479 PA 66
LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific)
LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EN95 PPE+PS (Asia Pacific)
Low heat, extrusion grade PPO/HIPS alloy.