Material Notes:
LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
1.42 g/cc
0.0513 lb/in³
ISO 1183
Moisture Absorption 0.970 %
0.970 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 204 MPa
29600 psi
ASTM D638
214 MPa
31000 psi
ISO 527
Elongation at Yield 2.1 %
2.1 %
ISO 527
Tensile Modulus 11.97 GPa
1736 ksi
1 mm/min; ISO 527
Flexural Strength 309 MPa
44800 psi
ISO 178
Flexural Modulus 9.88 GPa
1430 ksi
ASTM D790
10.24 GPa
1485 ksi
ISO 178
Izod Impact, Notched 2.77 J/cm
5.19 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1A
25.0 kJ/m²

@Temperature -40.0 °C
11.9 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
245 °C

@Thickness 3.20 mm
473 °F

@Thickness 0.126 in
unannealed; ASTM D648