Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.50 - 2.70 J/cm @Temperature 23.0 °C |
4.68 - 5.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Loxim 500 00V0 Polycarbonate/Acrylonitrile Butadiene Styrene Information provided by Loxim Industries |