Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.30 J/cm @Thickness 3.17 mm |
2.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Polyram PA310G8 Nylon 66, 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |