Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.22 J/cm | 4.16 ft-lb/in | ASTM D256 |
Plenco 08133 Polyester BMC, Compression Molded PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |