Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.02 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.02 J/cm

@Temperature -30.0 °C
3.78 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS
PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact
Izod Impact, Notched 2.02 J/cm
3.78 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA
High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load
Izod Impact, Notched 2.02 J/cm
3.78 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific)
High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load
Izod Impact, Notched 2.02 J/cm
3.78 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific)
High flow PPE+PA for under-the-hood and electrical applications. With mold release
Izod Impact, Notched 2.02 J/cm
3.78 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PS+PA
High flow PPE+PS+PA for under-the-hood and electrical applications. With mold release
Izod Impact, Notched 2.02 J/cm

@Temperature 23.0 °C
3.78 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific)
High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region.
Copyright © lookpolymers.com All Rights Reserved