Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.675 J/cm @Thickness 3.17 mm |
12.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers DIAMALOY 1012 ABS/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |