Mechanical Properties Metric English Comments
Izod Impact, Notched 6.407 J/cm
12.00 ft-lb/in
ASTM D256
Ovation Polymers UTTAP ES 10559 Polycarbonate Alloy
Polycarbonate Alloy – High temperature (HDT), high Impact, with excellent short and long term heat stability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative h..
Izod Impact, Notched 6.408 J/cm

@Temperature 23.0 °C
12.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
MRC Polymers NAXELLâ„¢ PC110VL Polycarbonate, Very Low MFR
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.