Ovation Polymers UTTAP ES 10559 Polycarbonate Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name UTTAP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers UTTAP ES 10559 Polycarbonate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate Alloy – High temperature (HDT), high Impact, with excellent short and long term heat stability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
50 mm/min; ASTM D638
Elongation at Break 40 %
40 %
50 mm/min; ASTM D638
Tensile Modulus 1.75 GPa
254 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 82.0 MPa
11900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.98 GPa
287 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.407 J/cm
12.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C

@Thickness 3.20 mm
275 °F

@Thickness 0.126 in
unannealed; ASTM D648