Polymer Property : Izod Impact, Notched = 1.902 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.015 J/cm

@Temperature 0.000 °C
1.902 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Petromont 1100 High Density Polyethylene Resin
Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b..
Izod Impact, Notched 1.015 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.902 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 1.015 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.902 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus