Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.015 J/cm @Temperature 0.000 °C |
1.902 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Izod Impact, Notched | 1.015 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.902 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 1.015 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.902 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |