Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.63 J/cm | 3.05 ft-lb/in | ASTM D256 |
I. Stern 728 High Gloss Medium Natural ABS Features:Super high glossEasy to colorApplicationsInjection moldingAppliancesInformation provided by I. Stern & Co. Inc. |