Features:Super high glossEasy to colorApplicationsInjection moldingAppliancesInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength 48.3 MPa
7000 psi
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Strength 68.6 MPa
9950 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 1.63 J/cm
3.05 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 86.1 °C
187 °F
ASTM D648