Mechanical Properties Metric English Comments
Izod Impact, Notched 1.61 J/cm
3.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Izod Impact, Notched 1.61 J/cm
3.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched 1.61 J/cm

@Temperature -30.0 °C
3.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PKN4775 PPE+PS
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Izod Impact, Notched 1.61 J/cm

@Temperature -30.0 °C
3.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Izod Impact, Notched 1.61 J/cm

@Temperature -30.0 °C
3.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Izod Impact, Notched 1.61 J/cm
3.02 ft-lb/in
ASTM D256
Cast Nylons Nycast® 12 Cast Nylon 12
NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara..
Izod Impact, Notched 1.61 J/cm
3.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.