Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.10678 - 0.80085 J/cm @Temperature 0.000 - 0.000 °C |
0.20004 - 1.5003 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.463 J/cm Grade Count:10 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.10678 - 0.80085 J/cm @Thickness 3.17 - 6.35 mm |
0.20004 - 1.5003 ft-lb/in @Thickness 0.125 - 0.250 in |
Average value: 0.463 J/cm Grade Count:10 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |