Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.715 J/cm @Temperature 23.0 °C |
1.34 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Forte™ 12HPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Izod Impact, Notched | 0.715 J/cm | 1.34 ft-lb/in | ASTM D256 |
BCC Products BC 8400 Urethane Casting BC8400 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8400 will exhibit high impact strength and yield thermoplastic-like parts. Some features i.. |