Material Notes:
BC8400 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8400 will exhibit high impact strength and yield thermoplastic-like parts. Some features include the following: mercury free, high impact strength, moderate heat resistance, no objectionable odor, excellent finishing properties, turns white upon cure, thermoplastic appearance, and longer mold life.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792-66
Brookfield Viscosity 190 cP
190 cP
Mixed
480 cP
480 cP
Part B
64 cP

@Temperature 23.9 °C
64 cP

@Temperature 75.0 °F
Part A
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D2566
Mechanical Properties Metric English Comments
Hardness, Shore D 72 - 78

@Temperature 23.9 °C
72 - 78

@Temperature 75.0 °F
ASTM D2240
Tensile Strength, Ultimate 36.72 MPa
5326 psi
ASTM D638
Elongation at Break 13.1 %
13.1 %
ASTM D638
Flexural Strength 60.5 MPa
8770 psi
ASTM D790
Flexural Modulus 1.730 GPa
250.9 ksi
ASTM D790
Izod Impact, Notched 0.715 J/cm
1.34 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 62.8 °C
145 °F
ASTM D648
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min

@Temperature 25.0 °C
0.500 - 1.00 hour

@Temperature 77.0 °F
demold time
Pot Life 3.0 min

@Temperature 24.0 °C
3.0 min

@Temperature 75.2 °F
gel time, 200g; ASTM 2471-71
Descriptive Properties Value Comments
Mix Ratio 1:1 by weight or volume