Polymer Property : Izod Impact, Notched = 1.15 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.694 - 1.15 J/cm
1.30 - 2.15 ft-lb/in
Average value: 0.943 J/cm Grade Count:16
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..