Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.529 J/cm | 0.991 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |