Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.96102 - 0.96102 J/cm @Temperature -28.9 - -28.9 °C |
1.8004 - 1.8004 ft-lb/in @Temperature -20.0 - -20.0 °F |
Average value: 0.961 J/cm Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |