Mechanical Properties Metric English Comments
Izod Impact, Notched 0.507 J/cm
0.950 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
Izod Impact, Notched 0.507 J/cm

@Temperature 23.0 °C
0.950 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Oxford Polymers 25GB-5GF-IM Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads
Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers.
Izod Impact, Notched 0.507 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.950 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ AT-10CF/15T-2S Acetal-Copolymer, Carbon Fiber Reinforced, PTFE/Silicone Lubricated  (disco
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.507 J/cm

@Thickness 3.17 mm
0.950 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 GF13 ML2 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz..
Izod Impact, Notched 0.507 J/cm

@Thickness 3.17 mm
0.950 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ABS GF30 HT 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.507 J/cm
0.950 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene
Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l..
Izod Impact, Notched 0.507 J/cm
0.950 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Dow H110-02N Polypropylene Resin
DOW H110-02N is intended for use in extrusion and thermoforming processes. It is especially suited for applications where improved melt strength and clarity are desired.Information provided by DowD..
Izod Impact, Notched 0.507 J/cm

@Temperature -40.0 °C
0.950 ft-lb/in

@Temperature -40.0 °F
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Izod Impact, Notched 0.507 J/cm

@Temperature 22.8 °C
0.950 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Amco PRIMATOP PP CO 350-10 RC Clarified Random Copolymer
Features:excellent processingimpactclarityanti-statApplications:rigid packaginghousewaresFormer A-Top Polymers product; part of Amco product line since 2013.