Material Notes:
Features:excellent processingimpactclarityanti-statApplications:rigid packaginghousewaresFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Melt Index of Compound 35 g/10 min

@Temperature 230 °C
35 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 32.1 MPa
4650 psi
50 mm/min; ASTM D638
Elongation at Yield 12.5 %
12.5 %
50 mm/min; ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
1.3 mm/min, 1% Secant; ASTM D790
Izod Impact, Notched 0.507 J/cm

@Temperature 22.8 °C
0.950 ft-lb/in

@Temperature 73.0 °F
ASTM D256