Mechanical Properties Metric English Comments
Izod Impact, Notched 0.454 J/cm
0.850 ft-lb/in
nominal; ASTM D256
S&E Specialty Polymers GPP6100-116C PP
Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus ..
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 HS YL030 Heat Stabilized
Availability: North AmericaForms: PelletsFeatures: Fast Molding Cycle and Good AdhesionAppearance: YellowTPCI# 10054102Information provided by TP Composites, Inc.
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 L N MB (Dry)
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co..
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 L N YL038MB
Availability: North AmericaForms: PelletsAdditive: Lubricant, UV Stabilizer and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Good UV Resistance and NucleatedAppeara..
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 L UV (Dry)
Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 LE BK (Dry)
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Low Extractables and NucleatedAppearance: BlackTPCI# 7..
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 X BN071 EL MB Nylon 6
Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Fast Molding Cycle, Good Processability, Lubricated and NucleatedTPCI# 1033102Information provided by TP Co..
Izod Impact, Notched 0.454 J/cm
0.850 ft-lb/in
ASTM D256
Techmer ES Plaslube® J-1/AF/15/TF/10 NAT PA66
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Plastiblend® PA6 L N BK MB Nylon 6
Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Fast Molding Cycle, Good Processability, Nucleated and LubricatedTPCI# 7970102Information provided by TP Co..
Izod Impact, Notched 0.454 J/cm

@Thickness 3.17 mm
0.850 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Plastiblend® PA6 L N BK002 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and Lubricant(4500 ppm)Features: Fast Molding Cycle, Good Processability, Nucleated and LubricatedAppearance: BlackTPCI# 1327102In..
Izod Impact, Notched 0.454 J/cm
0.850 ft-lb/in
ASTM D256
BCC Products MB 4000 RED Urethane Foundry Plank
MB4000 Red is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly ..
Izod Impact, Notched 0.454 J/cm
0.850 ft-lb/in
Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound
AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane..