Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.593 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-114 Compression Molded PEEK Compound, 40% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |