Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.310 - 2.51 J/cm | 0.580 - 4.70 ft-lb/in | Average value: 0.617 J/cm Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 22.8 °C |
0.580 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene MFP 22KA2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-96 Compression Molded PEEK Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled |