Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Hardness, Shore D 87
87
ASTM D2240
Tensile Strength 53.8 MPa
7800 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
Flexural Strain; ASTM D790
1.3 %
1.3 %
ASTM D638
Tensile Modulus 4.83 GPa
700 ksi
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Compressive Strength 165 MPa
24000 psi
10% Deformation; ASTM D695
Compressive Modulus 5.24 GPa
760 ksi
ASTM D695
Izod Impact, Notched 0.310 J/cm
0.580 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.11
0.11
ASTM D1894
Coefficient of Friction, Static 0.13
0.13
ASTM D1894
Thermal Properties Metric English Comments
Heat Distortion Temperature 254 °C
490 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 839 ohm-cm
839 ohm-cm
ASTM D257
Surface Resistance <= 842 ohm
<= 842 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black