Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.531 J/cm | 0.995 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Flam™ 0102 Natural PP Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |