Multibase Multi-Flam™ 0102 Natural PP Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Flam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flam™ 0102 Natural PP Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Melt Flow 2.96 g/10 min
2.96 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Strength 35.6 MPa
5170 psi
ASTM D790
Flexural Modulus 1.17 GPa
170 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 0.531 J/cm
0.995 ft-lb/in
73°F; ASTM D256
Gardner Impact 2.316 J
1.708 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
Unannealed; ASTM D648