Polymer Property : Izod Impact, Notched = 0.508 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.190 - 0.271 J/cm
0.356 - 0.508 ft-lb/in
Average value: 0.224 J/cm Grade Count:3
Overview of materials for Phenolic, Resole, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v..