Polymer Property : Izod Impact, Notched = 0.485 J/cm
Polymer Property :
Izod Impact, Notched =
0.485 J/cm
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Notched
>=
0.485
J/cm
>=
0.909
ft-lb/in
ASTM D256
Buckeye Polymers BP RPP 3505 GM BLK Polypropylene, Glass Filled
Information Provided by Buckeye Polymers, Inc.