Buckeye Polymers BP RPP 3505 GM BLK Polypropylene, Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 3505 GM BLK Polypropylene, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Melt Flow 6.0 - 12 g/10 min
6.0 - 12 g/10 min
ASTM D1238
Ash 28 - 34 %
28 - 34 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 40.49 MPa
>= 5872 psi
ASTM D638
Flexural Modulus >= 3.41 GPa
>= 495 ksi
ASTM D790
Izod Impact, Notched >= 0.485 J/cm
>= 0.909 ft-lb/in
ASTM D256