Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.240255 - 0.37373 J/cm @Temperature 0.000 - 0.000 °C |
0.450096 - 0.70015 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.463 J/cm Grade Count:6 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.240255 - 0.32034 J/cm @Temperature 0.000 - 0.000 °C |
0.450096 - 0.60013 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.274 J/cm Grade Count:4 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.240255 - 0.37373 J/cm @Temperature 0.000 - 0.000 °C |
0.450096 - 0.70015 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.330 J/cm Grade Count:6 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |