Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.226 J/cm | 0.422 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t.. |