Polymer Property : Izod Impact, Notched = 0.373 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.199 J/cm
0.373 ft-lb/in
ASTM D256
Plenco 2535 Phenolic, Granular, Compression Molded
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c..
Izod Impact, Notched 0.199 J/cm
0.373 ft-lb/in
ASTM D256
Plenco 3509 Phenolic, Granular, Compression Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..