Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.353 J/cm | 0.661 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30730 POM, 30% Mineral Reinforced |
|||
Izod Impact, Notched | 0.353 J/cm | 0.661 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30G15 POM, 15% Glass Fiber |
|||
Izod Impact, Notched | 0.353 J/cm | 0.661 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® N4040M1 Dimensional Stability Heat Resistance Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |