Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.156 - 0.188 J/cm | 0.292 - 0.352 ft-lb/in | Average value: 0.170 J/cm Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral Filled". Each property range of values reported is minimum and maximum values .. |