Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.325 J/cm @Temperature 23.0 °C |
0.609 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers |
|||
Izod Impact, Notched | 0.325 J/cm | 0.609 ft-lb/in | ASTM D256 |
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa.. |