Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.165 - 0.281 J/cm | 0.309 - 0.526 ft-lb/in | ASTM D256 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Izod Impact, Notched | 0.165 - 0.281 J/cm | 0.309 - 0.526 ft-lb/in | ASTM D256 |
3D Systems Accura® 50 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te.. |