Polymer Property : Charpy Impact, Notched = 83.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 17.5 J/cm²
83.3 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East)
Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized
Charpy Impact, Notched 17.5 J/cm²

@Temperature -30.0 °C
83.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East)
Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized