Polymer Property : Charpy Impact, Notched = 7.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP1 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP5 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Charpy Impact, Notched 1.47 J/cm²

@Temperature 22.8 °C
7.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP7 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Charpy Impact, Notched 1.47 J/cm²
7.00 ft-lb/in²
Eastman Tenite 131E-28 Cellulose Acetate  (discontinued **)
28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.