Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Charpy Impact, Notched | 1.47 J/cm² @Temperature 22.8 °C |
7.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Charpy Impact, Notched | 1.47 J/cm² | 7.00 ft-lb/in² | |
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |